Imperfections are a natural part of pottery, and many of these only manifest after a pot has been either bisque or glaze fired.
But you don’t need to throw a pot away just because of a minor imperfection!
In this episode, I talk about four very common imperfections in fired pottery and simple ways to fix them:
✔️Hairline cracks appearing in pieces of pottery after the bisque firing, in pieces of pottery that have been joined together
✔️A rough surface after a pot has been glaze-fired, created by a too-thin layer of ash glaze, e.g on the rim of a mug.
✔️A rough surface on the base of a pot caused by tiny pieces of kiln shelf sticking to it after the glaze firing.
✔️Bubbles in a glaze that become sharp once a pot has cooled after being glaze-fired.
You can watch the video version of this episode on YouTube.
-------------------------------
Resources for Potters:
⭐ Pottery Paperback Books available from Amazon
Free Pottery Guides:
🆓 Download the Free How to Make a Pottery Glaze Workbook (suitable for beginners):
🆓 Download the Free How to programme an Electric Kiln for bisque and stoneware glaze firings (includes full kiln firing schedule)
------------------------------------
Get every episode summarized
Each time Oxford Clay publishes, we email you a written briefing from the transcript — the topics, who appeared, and any specific claims, with the ad reads skipped.
Email me new episodesFree for 3 shows. No card needed.
Hosts & guests
No transcript yet
This episode has not been transcribed. Request it and it moves to the front of the queue.
More episodes
More from Oxford Clay

116. A Total Beginner's Guide to Making an Ash Glaze in Pottery
Oxford Clay

115. Where to Get Ash for Ash Glazing in Pottery
Oxford Clay

114. How to Make Your Kiln Firings More Efficient in Pottery
Oxford Clay

113. How to find Vegan-Friendly Glazing Brushes in Pottery
Oxford Clay